Clear eye opening 1.3micrometer-25 / 43Gbps EML with novel tensile-strained asymmetric QW absorption layer

Konferenz: ECOC 2009 - 35th European Conference on Optical Communication
20.09.2009 - 24.09.2009 in Vienna, Austria

Tagungsband: ECOC 2009

Seiten: 2Sprache: EnglischTyp: PDF

Persönliche VDE-Mitglieder erhalten auf diesen Artikel 10% Rabatt

Autoren:
Saito, Takeshi; Yamatoya, Takeshi; Morita, Yoshimichi; Ishimura, Eitaro; Watatani, Chikara; Aoyagi, Toshitaka; Ishikawa, Takahide (High Frequency & Optical Device Works, Mitsubishi Electric Corporation, 4-1 Mizuhara, Itami, Hyogo, 664-8641, Japan)

Inhalt:
We demonstrate 1.3micrometer-25/43Gbps EML with novel tensile-strained asymmetric quantum well absorption layer. Clear eye opening was achieved under high output power condition (>+5dBm) both before / after 10km normal SMF transmission up to 43Gbps.